    Improvement of Direct Evaluation Method for Internal Corrosion of Natural Gas Pipelines Containing H2S

    • 摘要: 为了确定H2S对天然气管道内腐蚀的影响,对NACE SP0110-2010标准提出的天然气管道内腐蚀直接评价方法(包括预评价、间接评价、直接评价、后评价四个环节)进行改进,即在该方法的间接评价环节引入了CO2-H2S腐蚀速率预测模型和积水概率参数,提高了推荐开挖点管道腐蚀程度的准确性。并以某含H2S天然气管道为例,对改进后的评价方法进行了演示。结果表明:根据间接评价(多相流腐蚀模拟计算),极严重腐蚀出现在管道前500 m处,23%管段的积水概率为1;根据直接评价(现场开挖),5个开挖点处管道均属于极严重腐蚀,最大腐蚀速率为0.337 mm/a,与间接评价的预测结果一致;根据后评价确定了管道再评估时间间隔为1 a。改进后评价方法对预测多相流含H2S天然气管道内腐蚀高危点具有一定的借鉴意义。

       

      Abstract: In order to determine the influence of H2S on internal corrosion of natural gas pipelines, the direct evaluation method for internal corrosion of natural gas pipelines proposed by NACE SP0110-2010 standard (including pre-evaluation, indirect evaluation, direct evaluation and post-evaluation) was improved by introducing CO2-H2S corrosion rate prediction model and ponding probability in the indirect evaluation of the method, which improved the accuracy of the corrosion degree of pipeline at recommended excavation points. Taking a natural gas pipeline containing H2S as an example, the improved evaluation method was demonstrated. The results show that according to indirect evaluation (multiphase flow corrosion simulation calculation), extremely severe corrosion occurred 500 m in front of the pipeline, and 23% of the pipeline sections had a ponding probability of 1. According to the direct evaluation (on-site excavation), the pipelines at all 5 excavation points were severely corroded, with a maximum corrosion rate of 0.337 mm/a, which was consistent with the predicted results of the indirect evaluation. According to the post-evaluation, the pipeline reassessment interval was determined to be 1 a. The improved evaluation method can provide certain reference for predicting high-risk corrosion points in multiphase flow natural gas pipelines containing H2S.

       

    /

    返回文章
    返回