CAI Suo-de, ZHAO Guo-xian, MIU Jian, LIU Si-jia. Anti-corrosion and Life Prediction of Artificial Migration Well Casing[J]. Corrosion & Protection, 2016, 37(4): 340-344. DOI: 10.11973/fsyfh-201604015
Citation: CAI Suo-de, ZHAO Guo-xian, MIU Jian, LIU Si-jia. Anti-corrosion and Life Prediction of Artificial Migration Well Casing[J]. Corrosion & Protection, 2016, 37(4): 340-344. DOI: 10.11973/fsyfh-201604015

Anti-corrosion and Life Prediction of Artificial Migration Well Casing

More Information
  • Received Date: October 28, 2015
  • By stimulating plugging soundness and plugging leakage, the corrosion inhibition of two kinds of inhibitor, HYF-01 and HSJ-JL-01, in different contents was evaluated, and the anti-corrosion life of N80 casing steel was calculated to choose the inhibitor and its best content to meet the requirement of anti-corrosion life of 15 years. The results show that the best content was 0.1% (mass fraction ) for both HYF-01 and HSJ-JL-01 in plugging soundness, and was 1.0% for both HYF-01 and HSJ-JL-01 in plugging leakage. Adding 0.5% and 1.0% HYF-01 could meet the requirement of anti-corrosion life of 15 years.
  • [1]
    胡士信,路民旭,杜艳霞. 管道交流腐蚀的新观点[J]. 腐蚀与防护,2010,31(6):419-424.
    [2]
    GUMMOW R A,WAKELIN R G,SEGALL S M. AC corrosion-a new challenge to pipeline integrity[C]//Corrosion 1998. Houston:NACE,1998:566.
    [3]
    梁明华,苗健. 一种咪唑啉缓蚀剂对油田用P110钢CO2腐蚀的缓蚀行为[J]. 腐蚀与防护,2013,34(5):395-398.
    [4]
    KERMANI M B,MORSHED A. Carbon dioxide corrosion in oil and gas production-a compendium[J]. Corrosion,2003,59(8):659-603.
    [5]
    LIU F G,DU M. Electro chemical behavior of Q235 steel in saltwater saturated with carbon dioxide based on new imidazoline derivative inhibitor[J]. Corrosion Science,2009,51:102-109.
    [6]
    RAMACHANDRAN S,AHN Y S,GREAVES M,et al. Development of high temperature,high pressure corrosion Inhibitor[C]//Corrosion 2006. Houston:NACE,2006:06377.
    [7]
    SY/T 7901-2001Metals materials-uniform corrosion-methods of laboratory immersion testing[S].
    [8]
    SY/T 5273-2014油田采出水处理用缓蚀剂性能指标及评价方法[S].
    [9]
    NACE Standard SP0775-2013Preparation,installation,analysis,and interpretation of corrosion coupons in oilfield operations[S].
    [10]
    秦开明,彭建国,李芳,等. N80套管钢CO2腐蚀缓蚀剂筛选及性能评价[J]. 管道技术与设备,2013(6):30-32.
    [11]
    王延,周永红,宋湛谦,等. 盐酸介质中脱氢松香咪唑啉缓蚀剂对Q235钢缓蚀性研究[J]. 腐蚀与防护,2002,19(6):247-249.
    [12]
    张永君,杨昌柱,彭珂如,等. 缓蚀剂与吸附作用[J]. 江西电力,1999,23(2):44-46.
    [13]
    李谦定,李恒娟,卢永斌. 咪唑啉季铵盐缓蚀剂的合成及应用性能评价[J]. 西安石油大学学报(自然科学版),2011,26(2):76-79.
    [14]
    宋莎莎,王斌. 咪唑啉季铵盐缓蚀剂的制备及性能研究[J]. 全面腐蚀控制,2009,23(4):15-17.
    [15]
    宋莎莎. 咪唑啉季铵盐缓蚀剂的制备及其性能研究[J]. 江苏化工,2008,36(4):15-17.
    [16]
    EI-AWADY A A,ABD-EI-NABEY B A,AZIZ S G. Kinetic-thermodynamic and adsorption isotherms analyses for the inhibition of the acid corrosion of steely cyclic and open-chain amines[J]. Journal of the Electrochemical Society,1992,139(8):2149-2154.
    [17]
    王建学,万建仓,沈慧. 钻井工程[M]. 北京:石油工业出版社,2008:218-220.
    [18]
    李平全. 油气田生产开发期套管的损坏原因分析油套管标准研究、油套管失效分析及典型案例-2[J]. 钢管,2006,35(5):53-59.
    [19]
    傅朝阳,刘小武,刘宏芳,等. 油套管腐蚀分析[J]. 四川化工与腐蚀控制,1999,2(4):4-7.
    [20]
    SY/T 5724-2008套管柱结构与强度设计[S].
    [21]
    SY/T 5322-2000套管柱强度设计方法[S].
    [22]
    韩志勇. 关于“套管柱三轴抗拉强度公式”的讨论[J]. 中国石油大学学报,2011,35(4):77-80.
    [23]
    李丹平,赵国仙,薛艳,等. 套管钢在模拟碳酸盐岩环境中的腐蚀寿命预测[J]. 热加工工艺,2013,42(12):236-238.
    [24]
    Q/HS14015-2012海上油气井油管和套管防腐设计指南[S].

Catalog

    Article views (10) PDF downloads (2) Cited by()

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return