Advanced Search

    column
    Corrosion Electrochemical Behavior of X80 Pipeline Steel in Simulated Dagang Soil Solution
    HUANG Feng, LIU Jing, LIN Chao, QU Yan-miao, YU Lu, CHENG Ji-hao
    2010, 31(2): 95-99.
    Abstract PDF
    Adsorption and Inhibition Effect of Tween40 on Cold Rolled Steel in HCl Solution
    BAI Wei, LI Xiang-hong, DENG Shu-duan, KEN Sheng-ye, LI Lei
    2010, 31(2): 100-102.
    Abstract PDF
    Aging Behavior of Epoxy Molding Compound for Electronic Components in Hydrothermal Environment
    ZHANG Jin-feng, LIU Hui-cong, LI Wei-ping, ZHU Li-qun
    2010, 31(2): 103-106.
    Abstract PDF
    Fabrication and Characterization of Stable Super Hydrophobic Cupric Oxide Films
    LIU Hong-qin, XU Wen-guo, WANG Yan-bin, LU Shi-xiang
    2010, 31(2): 107-110.
    Abstract PDF
    Under-deposit Occluded Cell Corrosion Inhibition Mechanism of N80 Steel in NaCl Solution Added with Sodium Laurate
    ZHU Yuan-liang, JI E-yu, QIU Yu-bing, GUO Xing-peng
    2010, 31(2): 111-114.
    Abstract PDF
    Effect of HEDP on Corrosion Behavior of 1Cr18Ni9Ti in HNO3 Cleaning System
    GONG Min, WEI Wei, ZHANG Peng, LIN Xiu-zhou, KANG Wu, ZHANG dong, ZHAO Chao-kang
    2010, 31(2): 115-117.
    Abstract PDF
    A Sulphuric Solution Inhibitor Containing Dithiocarbamate and Its Anti-corrosion Effect on Copper
    LIAO Qiang-qiang, YUE Zhong-wen, SHEN Xi, YU Zhen-yin, LI Yi-jiu, ZHOU Qi
    2010, 31(2): 118-120.
    Abstract PDF
    Electrochemical Behavior of AZ31 Magnesium Alloy in Different Electrolytes
    YAO Yu-fen, CHEN Chang-guo, ZHANG Pei-hong, LIU Yu-ping, LI Lei-guang, LEI Shu
    2010, 31(2): 121-124.
    Abstract PDF
    Effects of Bath Temperature on Electroless Ni-P Plating of AZ31 Magnesium Alloy
    SHANG Shu-zhen, LU Gui-min, ZHAO Zu-xin, WAN Yi-jun
    2010, 31(2): 125-127.
    Abstract PDF
    Effect of Microbe in Urban Sewage on Corrosion Resistance of Carbon Steel
    GONG Li-hua, CUI Jing-hai, QI Xia
    2010, 31(2): 128-130.
    Abstract PDF
    Influence of Thickness of Micro-arc Oxidation Coatings on Corrosion Resistance of AZ91D Magnesium Alloy
    ZHANG Yong, CHEN Yue-liang, YU Da-zhao, ZHANG Tai-feng, ZHU Wu-feng
    2010, 31(2): 131-134.
    Abstract PDF
    Parameter Optimization and High Temperature Resistance of Arc Sprayed Coatings with Cored Wires
    ZHANG Guang-ming, WANG Yong, CHENG Yi-yuan
    2010, 31(2): 135-138.
    Abstract PDF
    Structure and Corrosion Resistance of Galvanized Steel Sheets Treated by Environmental Friendly Passivation Solution
    ZHONG Bin, XU Xiao-lian, CHEN Yi-qing, AI Fang-fang, XIAO Yu, XU Cheng-ming, WANG Yong-ming, LI Feng
    2010, 31(2): 139-141.
    Abstract PDF
    Composite Passivation Technology for Galvanized Steel
    YI De-lian, WANG Jing, LI Yu-peng, LIU Min, WU Lin, PANG Kuan, DOU Bing-qian, LI Min-min
    2010, 31(2): 142-145.
    Abstract PDF
    Metal Corrosion Inhibitors in Chlorine Dioxide Solution
    SHEN Jing-jing, WANG Kui-tao, LIU Yan1, XU Jun-jie, ZHENG Zhi-jun, ZHANG Bing-zhu
    2010, 31(2): 146-148.
    Abstract PDF
    Research Status of Corrosion Behavior of 316LSS and 2205DSS
    LIU Zuo-jia
    2010, 31(2): 149-153.
    Abstract PDF
    Failure Reasons of Heat Shrinkable Sleeve for 3PE Pipeline
    CHEN Hong-yuan, LIU Ling-li, ZHAO Jun, HOU Yu, WANG De-zeng, HAN Zhong-qin
    2010, 31(2): 154-157.
    Abstract PDF
    Preparation of Zirconate Chemical Conversion Film on Aluminium Alloy
    ZHOU Qi, ZHANG Chun-li, ZHANG Guang-sen
    2010, 31(2): 158-160.
    Abstract PDF
    Corrosion Behavior of Glass Flake Coating in Flue Gas Desulphurization System
    ZHANG Yi-gang, LI Shu-ying
    2010, 31(2): 161-163.
    Abstract PDF
    A Composite Inhibitor for Anti-scale and Auti-corrosion in Water Treatment
    WANG Jun-feng, DONG Ji-xian, GUO Rui
    2010, 31(2): 164-166.
    Abstract PDF
    Corrosion Behaviors of Three Metal Materials in Autoclave Containing Saline Medium
    WANG Guan-jun, LIU Jing-shu, ZHANG Jie
    2010, 31(2): 167-169.
    Abstract PDF
    Application of Corrosion Monitoring Technology in the Production System of Tahe Oilfield
    ZHANG Jian, LU Rui-dian, LI Xin-yong, LIU Ji-ning, GAO Shu-hong
    2010, 31(2): 170-171.
    Abstract PDF
    Application of An Environmental-friendly Powder Coating in OCTG
    HU Jian-xiu, ZHANG Gui-xin, WANG Qian, LI Wen-tong, ZHANG Yan-dong
    2010, 31(2): 172-173.
    Abstract PDF
    Application of Epoxy Modified Furan Resin to Dry-absorption Workshop in Sulfuric Acid Factory
    ZHANG Hong-chen
    2010, 31(2): 174-175.
    Abstract PDF
    Failure Analysis for the Rupture of Segregator Pipeline in Diesel Hydrofining Unit
    CHEN Xu, WANG Yu-shun, DING Yi, MA Li-qun
    2010, 31(2): 176-178.