Advanced Search

    column
    Corrosion Behavior of Ferrous Metals Exposed to the Yangtse River in Wuhan of China
    HUANG Gui-qiao, YANG Zhao-hui, ZHOU Xue-jie, HAN Bing
    2009, 30(10): 675-677.
    Abstract PDF
    Relationship between Hydrogen-induced Additive Stress and Threshold Cracking Stress for a High-strength Steel
    LI Hui-lu, YU Zhu-huan, LI Ying, CHU Wu-yang, QIAO Li-jie
    2009, 30(10): 678-683.
    Abstract PDF
    Intergranular Corrosion Susceptibility of Welded Joint of Stainless Steels
    MENG Wei, YANG Rui-cheng, SHU Jun, HU Tian-lei, NIU Shao-rui
    2009, 30(10): 684-687.
    Abstract PDF
    Oxidation Resistance of Nanocrystalline Cu-Si Alloys at High Temperatures
    SU Yong, FU Guang-yan, LIU Qun
    2009, 30(10): 688-692.
    Abstract PDF
    Effect of Ca2+ Concentration on Protection Properties of X65 Steel Corrosion Scale
    DING Chen, GAO Ke-wei, CHEN Chang-feng
    2009, 30(10): 693-696.
    Abstract PDF
    Effect of Reduction Methods on Ag/AgX Reference Electrodes Prepared by Thermal Dip-coating Method
    YIN Peng-fei, XUE Gui-lin, WANG Jun-tao, XU Li-kun, HOU Wen-tao
    2009, 30(10): 697-700.
    Abstract PDF
    Effect of Cathodic Polarization on the Susceptibility to Hydrogen Embrittlement of 907 Steel
    YANG Zhao-yan, YAN Yong-gui, MA li, ZHANG Gui-ling
    2009, 30(10): 701-703.
    Abstract PDF
    Effect of Si on Corrosion Resistance of Iron-based Alloys in Molten Zinc
    ZHANG Yi, LI Hong-bo, LIU Jun-you
    2009, 30(10): 704-707.
    Abstract PDF
    Corrosion Behavior of Nickel Based Alloy 825 in High Temperature and High Pressure H2S/CO2 Environments
    GE Lei, CHEN Chang-feng, ZHENG Shu-qi, CAI Xiao-wen
    2009, 30(10): 708-710.
    Abstract PDF
    Effect of Dissolved Oxygen on Corrosion of 20R Steel in Bio-diesel Reactor Raw Mixture
    LIU Jie, FANG Yan-kai
    2009, 30(10): 711-712.
    Abstract PDF
    Effect of Copper on Corrosion Resistance of Cr-Mn Stainless Steel
    JIN Yun-xue, ZHANG Yan, DAI An-lun, GUO Yu-hang, FU Xue-hui
    2009, 30(10): 713-716.
    Abstract PDF
    A New Antirusting Agent with Water-soluble Polymer for Steels
    LI Ming-xian, ZHANG De-jun, WU Wen-xiang
    2009, 30(10): 717-720.
    Abstract PDF
    Inhibitor of Naphthenic Acid Corrosion in Atmospheric and Vacuum Distillation Unit
    HUANG Ben-sheng, LI Hui, LIU Qing-you, MA Xin, WANG Yan
    2009, 30(10): 721-723.
    Abstract PDF
    Effect of Impact Power on Corrosive Wear of Medium Carbon Alloy Steel
    SHEN Chao-ying, ZHU Kai, WANG Shou-zhong
    2009, 30(10): 724-726.
    Abstract PDF
    Development Status of Chromium-free Conversion Coating Technology
    HU Hui-li, CHEN Li-jiao
    2009, 30(10): 727-731.
    Abstract PDF
    Research and Development Status of the Environmental Corrosion Inhibitors
    WANG Guo-rui, LIU Zheng, LIU Er-xi, LIU Bao-yu
    2009, 30(10): 732-737.
    Abstract PDF
    Advances in Research on High Temperature Anti-oxidation Coatings of C/C Composites
    CHEN Shao-jie, ZHANG Jiao-qiang, GUO Yin-ming
    2009, 30(10): 738-741.
    Abstract PDF
    Technical Optimization and Corrosion Resistance of Cerium Conversion Film
    HE Ge-ping, HE Yong-ning, XU Qi-ming
    2009, 30(10): 742-744.
    Abstract PDF
    Implantation Technique of Corrosion Inhibitors for Air Injection Enhanced Oil Recovery
    ZHOU Quan, REN Shao-ran, YU Hong-min, DONG Li-shan, DING Gang, LIN Wei-min, GAO Hai-tao
    2009, 30(10): 745-746.
    Abstract PDF
    Anticorrosion Ability of A New-type Water-based Drawing Lubricant for Steel Cord
    RUI Bin
    2009, 30(10): 747-748.
    Abstract PDF
    Corrosion and Protection of the Bearing Boat Float Bridge in the Yellow River
    SHAO Jie, SUN Zhi-wei, CAO Rui-Xiang
    2009, 30(10): 749-750.
    Abstract PDF
    Scaling Reasons and Prevention Measures of Heat Exchanger at the Top of Atmospheric Column
    ZHAO Min, KANG Qiang-li, CUI Ke-long, KONG Zhao-hui, XU Yi
    2009, 30(10): 751-752.
    Abstract PDF
    A New Technology of Normal Temperature Oxidation for Steel Parts
    HUANG Yan-song, MA Jun-wen, WANG Bin
    2009, 30(10): 753-755.
    Abstract PDF
    Corrosion Resistance of PVDF in the Inner Wall of Carbon Steel Hot Water Tank
    LI Yong, HU Ming-fu
    2009, 30(10): 756-757.
    Abstract PDF
    Failure Analysis and Treatment of Aluminized Water Wall Tubes
    XU Hong
    2009, 30(10): 758-760.
    Abstract PDF